主要應用:
汽車部件,包括燃油、傳動及發(fā)動機系統(tǒng),可減輕重量、降低成本并提供長時間的使用壽命;
芯片組和插座、杯體焊接支座;
片狀電容器、開關及微型喇叭、制作高密度的印刷電路板連接器;
用于耐磨要求極高的場合,例如無潤滑軸承、密封、軸承隔離環(huán)和往復開壓縮機零件;
連接器、控制器、傳感器、馬達及其它關鍵電子部件. 聯(lián)系人;李生18219005688
DuPont Performance Polymers Zytel? HTN52G35HSL BK420 PA6T/XT-GF35 | |||
---|---|---|---|
Categories: | Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 35% Glass Fiber Reinforced | ||
Material Notes: |
35% Glass Reinforced, PPA, High Performance Polyamide
Information provided by DuPont Performance Polymers |
||
Vendors: |
Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |
||
|
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Density | 1.57 g/cc | 0.0567 lb/in3 | DAM; ISO 1183 | ||
Water Absorption |
3.60 % @Thickness 2.00 mm |
3.60 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 | ||
Moisture Absorption |
1.00 % @Thickness 2.00 mm |
1.00 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 | ||
Linear Mold Shrinkage, Flow | 0.00200 cm/cm | 0.00200 in/in | DAM; ISO 294-4, 2577 | ||
0.00600 cm/cm | 0.00600 in/in | DAM; ISO 294-4, 2577 | |||
Mechanical Properties | Metric | English | Comments | ||
Tensile Strength at Break | 230 MPa | 33400 psi | 50%RH; ISO 527-1/-2 | ||
240 MPa | 34800 psi | DAM; ISO 527-1/-2 | |||
Elongation at Break | 2.00 % | 2.00 % | 50%RH; ISO 527-1/-2 | ||
2.30 % | 2.30 % | DAM; ISO 527-1/-2 | |||
Tensile Modulus | 15.0 GPa | 2180 ksi | DAM; ISO 527-1/-2 | ||
15.5 GPa | 2250 ksi | 50%RH; ISO 527-1/-2 | |||
Flexural Modulus | 13.2 GPa | 1910 ksi | DAM; ISO 178 | ||
Izod Impact, Notched (ISO) ![]() |
12.0 kJ/m2 @Temperature 23.0 °C |
5.71 ft-lb/in2 @Temperature 73.4 °F |
DAM; ISO 180/1A | ||
13.0 kJ/m2 @Temperature -40.0 °C |
6.19 ft-lb/in2 @Temperature -40.0 °F |
DAM; ISO 180/1A | |||
Charpy Impact Unnotched ![]() |
8.00 J/cm2 @Temperature -30.0 °C |
38.1 ft-lb/in2 @Temperature -22.0 °F |
DAM; ISO 179/1eU | ||
8.50 J/cm2 @Temperature 23.0 °C |
40.4 ft-lb/in2 @Temperature 73.4 °F |
DAM; ISO 179/1eU | |||
Charpy Impact, Notched ![]() |
1.20 J/cm2 @Temperature 23.0 °C |
5.71 ft-lb/in2 @Temperature 73.4 °F |
DAM; ISO 179/1eA | ||
1.20 J/cm2 @Temperature -30.0 °C |
5.71 ft-lb/in2 @Temperature -22.0 °F |
DAM; ISO 179/1eA | |||
Electrical Properties | Metric | English | Comments | ||
Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | DAM; IEC 60093 | ||
Thermal Properties | Metric | English | Comments | ||
Melting Point | 300 °C | 572 °F | first heat; DAM; ISO 11357-1/-3 | ||
Deflection Temperature at 0.46 MPa (66 psi) | 285 °C | 545 °F | DAM; ISO 75-1/-2 | ||
Deflection Temperature at 1.8 MPa (264 psi) | 265 °C | 509 °F | DAM; ISO 75-1/-2 | ||
Flammability, UL94 ![]() |
HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | ||
HB @Thickness 0.850 mm |
HB @Thickness 0.0335 in |
DAM; IEC 60695-11-10 | |||
Flame Spread |
29.0 mm/min @Thickness 1.00 mm |
1.14 in/min @Thickness 0.0394 in |
Burning rate; ISO 3795 (FMVSS 302) | ||
Processing Properties | Metric | English | Comments | ||
Melt Temperature | >= 320 °C | >= 608 °F | |||
325 °C | 617 °F | Optimum | |||
<= 330 °C | <= 626 °F | ||||
Mold Temperature | >= 140 °C | >= 284 °F | |||
150 °C | 302 °F | Optimum | |||
<= 160 °C | <= 320 °F | ||||
Drying Temperature |
100 °C @Time 21600 - 28800 sec |
212 °F @Time 6.00 - 8.00 hour |
|||
Moisture Content | 0.100 % | 0.100 % | |||
De |
|||||
Drying Recommended | yes | ||||
Part Marking Code | >PA6T/XT-GF45< | ISO 11469 | |||
>PPA-GF45< | SAE J1344 | ||||
Processing | Injection Molding | ||||
Regional Availability | Asia Pacific | ||||
Europe | |||||
Global | |||||
Near East/Africa | |||||
North America | |||||
South and Central America | |||||
Resin Identification | PA6T/XT-GF45 | ISO 1043 | |||
Special characteristics | Heat stabilized or stable to heat |
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb'sterms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
DuPont Performance Polymers Zytel? HTN51G45HSL NC010 PA6T/XT-GF45
DuPont Performance Polymers Zytel? HTN51G35HSLR BK420J PA6T/XT-GF35
DuPont Performance Polymers Zytel? HTN51G35HSLR BK420 PA6T/XT-GF35
DuPont Performance Polymers Zytel? HTN51G35HSL NC010 PA6T/XT-GF35